The crack initiates at stress concentration point in the root of weld, where has much more martenite, carbide and inclusion, and the serious hydrogen segregation.
裂纹在焊缝根部应力集中,该马氏体含量比大,碳化物及夹杂物多,氢的偏聚现象严重。
The crack initiates at stress concentration point in the root of weld, where has much more martenite, carbide and inclusion, and the serious hydrogen segregation.
裂纹在焊缝根部应力集中,该马氏体含量比大,碳化物及夹杂物多,氢的偏聚现象严重。