The dehydriding temperature and dehydriding capacity were evaluated by differential scanning calorimeter (DSC) and thermogravimetric analysis (TG).
运用差热分析和热重分析材料的放温度和放量进行了测试。
The dehydriding temperature and dehydriding capacity were evaluated by differential scanning calorimeter (DSC) and thermogravimetric analysis (TG).